NAGIOS: RODERIC FUNCIONANDO

Bond strength of dental nanocomposites repaired with a bulkfill composite

Repositori DSpace/Manakin

IMPORTANT: Aquest repositori està en una versió antiga des del 3/12/2023. La nova instal.lació está en https://roderic.uv.es/

Bond strength of dental nanocomposites repaired with a bulkfill composite

Mostra el registre parcial de l'element

dc.contributor.author Koç Vural, Uzay es
dc.contributor.author Kerimova, Leyla es
dc.contributor.author Baltacioglu, ?smail H. es
dc.contributor.author Kiremitç, Arlin es
dc.date.accessioned 2017-07-18T11:55:33Z
dc.date.available 2017-07-18T11:55:33Z
dc.date.issued 2017 es
dc.identifier.citation Koç Vural, Uzay ; Kerimova, Leyla ; Baltacioglu, ?smail H. ; Kiremitç, Arlin. Bond strength of dental nanocomposites repaired with a bulkfill composite. En: Journal of Clinical and Experimental Dentistry, 9 3 2017: 437-442 es
dc.identifier.uri http://hdl.handle.net/10550/59594
dc.description.abstract The aim of this study was to analyze the bond strength of aged resin based nanocomposites repaired with the same and bulk fill composites. Seventy-two disc shaped resin composites consisted of three different nanocomposite resins (Filtek Ultimate/FU, Herculite XRV Ultra/HXRV, and Reflectys/R) were produced. After storing the samples for 8 weeks in distilled water, each material was combined with the same material or the bulk-fill composite resin system (Filtek Ultimate+Filtek Ultimate/Group-1; Filtek Ultimate+Tetric BF/Group-2; Herculite XRV+Herculite XRV/Group-3; Herculite XRV+Tetric BF/ Group-4; Reflectys+Reflectys/Group 5; Reflectys+Tetric BF/Group-6), for repair. Then specimens were subjected to shear bond strength testing(SBS), and the debonded surfaces were examined. There was a significant difference among three materials(repaired with itself+bulk fill) for SBS testing values (p=0.001). FU and R were found to be similar, while HXRV was significantly different from them. A significant difference between group-1 and 2 (p=0.006) was detected, while there were no differences between group 3 and 4 (p= 0.142), and 5 and 6 (p=0.346). Among the six groups, repair SBS testing values with TBF were higher than repair with itself except for FU. The bulk-fill repaired materials showed higher bond strength except for FU, which showed the highest SBS value when repaired with itself. An increased incidence of adhesive fracture was observed at low strengths. es
dc.title Bond strength of dental nanocomposites repaired with a bulkfill composite es
dc.type journal article es_ES
dc.subject.unesco UNESCO::CIENCIAS MÉDICAS es
dc.identifier.doi 10.4317/jced.53501 es
dc.type.hasVersion VoR es_ES

Visualització       (566.4Kb)

Aquest element apareix en la col·lecció o col·leccions següent(s)

Mostra el registre parcial de l'element

Cerca a RODERIC

Cerca avançada

Visualitza

Estadístiques