Morales Chávez, Mariana Carolina; Nualart Grollmus, Zacy Carola
|
|
Aquest document és un/a article, creat/da en: 2014
|
|
|
|
Objectives: The aim of this research is to evaluate the retention of sealants of resin and resin-modified ionomeric
glass pits and fissures, on first permanent molars of special patients.
Material and Methods: The sample was comprised by 32 children. The ages were between 7 and 18 years. The
sealing procedure was made with the relative isolation of the molars to be sealed, through the use of cotton rolls.
Two molars were sealed with Clinpro Sealant 3M Dental and the others with Vitremer. Checking of the sealants
was made after 3 and 6 months of their placement, evaluating with 3 values: TR: Totally Restrained; PR: Partially
Restrained; and CL: Completely Lost.
Results: 67.18% of the resinous sealants, and 70.31% of the glass ionomer sealants were successful after three
months. After six months, 57.81% of the resin-based sealants and 51.56% of the glass ionomer sealants were successful. When performing the Chi-square statistical analysis (
P
<0.05) no statistical significance was observed after
6 months.
Conclusions: The retention of the resin sealant was similar to that of the glass ionomer cement at the end of six
months and the retention of sealants on maxillary teeth was higher than on mandibular teeth.
|
|