NAGIOS: RODERIC FUNCIONANDO

In vitro comparative study on the friction of stainless steel wires with and without Orthospeed (JAL 90458) on an inclined plane

Repositori DSpace/Manakin

IMPORTANT: Aquest repositori està en una versió antiga des del 3/12/2023. La nova instal.lació está en https://roderic.uv.es/

In vitro comparative study on the friction of stainless steel wires with and without Orthospeed (JAL 90458) on an inclined plane

Mostra el registre parcial de l'element

dc.contributor.author Alió Sanz, Juan José es
dc.contributor.author Claros-Stucchi, Miguel es
dc.contributor.author Albaladejo Martínez, Alberto es
dc.contributor.author Iglesias-Conde, Carmen es
dc.contributor.author Alvarado Lorenzo, Alfonso es
dc.date.accessioned 2016-05-26T09:33:02Z
dc.date.available 2016-05-26T09:33:02Z
dc.date.issued 2016 es
dc.identifier.citation Alió Sanz, Juan José ; Claros-Stucchi, Miguel ; Albaladejo Martínez, Alberto ; Iglesias-Conde, Carmen ; Alvarado Lorenzo, Alfonso. In vitro comparative study on the friction of stainless steel wires with and without Orthospeed (JAL 90458) on an inclined plane. En: Journal of Clinical and Experimental Dentistry, 2016, Vol. 8, No. 2: 141-145 es
dc.identifier.uri http://hdl.handle.net/10550/53784
dc.description.abstract Background: During the treatment of orthodontics, in the mechanics of slide, there takes place friction, which they reduce the slide of the arch across bracket. Therefore, clinical there takes place an increase of the time of treatment. There are different the technologies that try to reduce this friction, as the self-ligating braces. The purpose of this study was to research the in vitro behavior of JAL 90458 as a buffering agent which reduces friction between brackets and stainless steel arch wires of different cross sections and sizes. Material and Methods: Three types of stainless steel wires with different cross sections and three types of ligatures were used with and without JAL 90458 to measure the friction according to the time and distance traveled by the brackets on an inclined plane with two angulations. The Kruskal-Wallis one-way analysis of variance by ranks was applied to determine the degree of friction between the group using and the group not using the product ( P ≤ .05). Results: Separate analysis of the arch wires, ligatures and angulation with and without the compound revealed statistically significant differences between the groups, showing that friction was reduced significantly when JAL 90458 was used ( P ≤ .01). The 0.021x0.025” arch wires and the arch wires attached using elastic ligatures produce the least resistance to sliding among all of those analyzed when the product was not used ( P ≤ .05). Conclusions: The results show that JAL 90458 reduces friction independently of arch wire cross section, type of ligature and angulation of the measuring instrument. en_US
dc.subject Odontología es
dc.subject Ciencias de la salud es
dc.title In vitro comparative study on the friction of stainless steel wires with and without Orthospeed (JAL 90458) on an inclined plane es
dc.type journal article es_ES
dc.subject.unesco UNESCO::CIENCIAS MÉDICAS es
dc.type.hasVersion VoR es_ES

Visualització       (906.8Kb)

Aquest element apareix en la col·lecció o col·leccions següent(s)

Mostra el registre parcial de l'element

Cerca a RODERIC

Cerca avançada

Visualitza

Estadístiques