Sealing efficacy of mineral trioxide aggregate with and without nanosilver for root end filling: an in vitro bacterial leakage study

Repositori DSpace/Manakin

IMPORTANT: Aquest repositori està en una versió antiga des del 3/12/2023. La nova instal.lació está en https://roderic.uv.es/

Sealing efficacy of mineral trioxide aggregate with and without nanosilver for root end filling: an in vitro bacterial leakage study

Mostra el registre parcial de l'element

dc.contributor.author Eskandarinezhad, Mahsa es
dc.contributor.author Shahvaghar-Asl, Naiemeh es
dc.contributor.author Sharghi, Reza es
dc.contributor.author Shirazi, Sajjad es
dc.contributor.author Shakouie, Sahar es
dc.contributor.author Salem Milani, Amin es
dc.contributor.author Balaei, Esrafil es
dc.date.accessioned 2017-05-10T11:18:37Z
dc.date.available 2017-05-10T11:18:37Z
dc.date.issued 2017 es
dc.identifier.citation Eskandarinezhad, Mahsa ; Shahvaghar-Asl, Naiemeh ; Sharghi, Reza ; Shirazi, Sajjad ; Shakouie, Sahar ; Salem Milani, Amin ; Balaei, Esrafil. Sealing efficacy of mineral trioxide aggregate with and without nanosilver for root end filling: an in vitro bacterial leakage study. En: Journal of Clinical and Experimental Dentistry. 2017. Vol. 9, no. 1: 27 es
dc.identifier.uri http://hdl.handle.net/10550/58468
dc.description.abstract Various materials have been added to mineral trioxide aggregate to enhance its properties. This study was aimed to compare the sealing efficacy of MTA with and without nanosilver using bacterial leakage approach. Seventy canine teeth were prepared and obturated. Then, after apical resection, the root-end cavities were prepared by ultrasonic retrotips. Teeth were randomly divided into 4 groups containing two experimental groups (n=30) and two negative and positive controls (n=5). In group 1 and 2, root-end cavities were respectively filled with MTA and MTA with nanosilver (by 1% weight). Leakage assessment was carried out by bacterial leakage apparatus with Enterococcus faecalis species. Leakage comparison between experimental groups was done using Mann-Whitney test by Spss 16 software at significancy level of 0.05. The median bacterial leakages for MTA and MTA with nanosilver were 19 and 2, respectively. The mean bacterial leakages for MTA and MTA with nanosilver were 30.06±28.67 and 9.66±14.25, respectively. Mann-Whitney test indicated that there was a significant difference in bacterial leakage day between two experimental groups (P=0.002). Based on the findings of this in-vitro bacterial leakage study, adding nanosilver to MTA decreased its sealing ability. en_US
dc.subject Odontología es
dc.subject Ciencias de la salud es
dc.title Sealing efficacy of mineral trioxide aggregate with and without nanosilver for root end filling: an in vitro bacterial leakage study es
dc.type journal article es_ES
dc.subject.unesco UNESCO::CIENCIAS MÃ DICAS es
dc.type.hasVersion VoR es_ES

Visualització       (1.544Mb)

Aquest element apareix en la col·lecció o col·leccions següent(s)

Mostra el registre parcial de l'element

Cerca a RODERIC

Cerca avançada

Visualitza

Estadístiques