NAGIOS: RODERIC FUNCIONANDO

The effect of incorporating different concentrations of chlorhexidine digluconate on the degree of conversion of an experimental adhesive resin

Repositori DSpace/Manakin

IMPORTANT: Aquest repositori està en una versió antiga des del 3/12/2023. La nova instal.lació está en https://roderic.uv.es/

The effect of incorporating different concentrations of chlorhexidine digluconate on the degree of conversion of an experimental adhesive resin

Mostra el registre parcial de l'element

dc.contributor.author Moharam, Lamiaa M. es
dc.contributor.author Salem, Haidy-Nabil es
dc.contributor.author Elgamily, Hanaa-Mahmoud es
dc.date.accessioned 2018-05-23T09:27:01Z
dc.date.available 2018-05-23T09:27:01Z
dc.date.issued 2018 es
dc.identifier.citation Moharam, Lamiaa M. ; Salem, Haidy-Nabil ; Elgamily, Hanaa-Mahmoud. The effect of incorporating different concentrations of chlorhexidine digluconate on the degree of conversion of an experimental adhesive resin. En: Journal of Clinical and Experimental Dentistry, 10 4 2018: 371-377 es
dc.identifier.uri http://hdl.handle.net/10550/66368
dc.description.abstract The aim of this study was to evaluate the effect of chlorhexidine digluconate incorporation on the degree of conversion of an experimental adhesive resin. The experimental resin was prepared from 70 wt% bisphenol A glycerolate dimethacrylate, 30 wt% hydroxyethyl methacrylate, silanized SiO2 nanofillers, 0.5% of camphorquinone and ethyl 4-dimethylaminebenzoate (binary photo-initiator system). Five chlorhexidine digluconate concentrations (0, 0.5, 1, 2 and 4 wt%) were then incorporated into the experimental resin. Thirty Potassium Bromide pellets were prepared then divided into six groups (n=5/group), repre¬senting the tested adhesive resins (Single Bond 2, 0, 0.5, 1, 2 and 4 wt% chlohexidine-incorporated experimental adhesive resins), that were applied to the pellets without light-curing (uncured specimens). Another 30 pellets were prepared and treated with the previous materials then light-cured using LED light-curing device (cured specimens). Degree of conversion of the uncured and the cured specimens were evaluated using FTIR analysis. Adper Single Bond 2 showed the highest degree of conversion mean values followed by 0.5 wt% chlorhexidine concentration then 2 wt% followed by 4 wt% then 1 wt% concentrations, while 0 wt% concentration showed the lowest mean values. Chlorhexidine digluconate had slight significant influence on the efficiency of polymerization of the experimental adhesive resin. es
dc.title The effect of incorporating different concentrations of chlorhexidine digluconate on the degree of conversion of an experimental adhesive resin es
dc.type journal article es_ES
dc.subject.unesco UNESCO::CIENCIAS MÉDICAS es
dc.identifier.doi 10.4317/jced.54391 es
dc.type.hasVersion VoR es_ES

Visualització       (431.3Kb)