NAGIOS: RODERIC FUNCIONANDO

Interfacial fracture toughness of universal adhesive systems treated with an antioxidant

Repositori DSpace/Manakin

IMPORTANT: Aquest repositori està en una versió antiga des del 3/12/2023. La nova instal.lació está en https://roderic.uv.es/

Interfacial fracture toughness of universal adhesive systems treated with an antioxidant

Mostra el registre parcial de l'element

dc.contributor.author Samimi, Pouran es
dc.contributor.author Nazem, Reihaneh es
dc.contributor.author Shirban, Farinaz es
dc.contributor.author Khoroushi, Maryam es
dc.date.accessioned 2018-07-30T09:38:00Z
dc.date.available 2018-07-30T09:38:00Z
dc.date.issued 2018 es
dc.identifier.citation Samimi, Pouran ; Nazem, Reihaneh ; Shirban, Farinaz ; Khoroushi, Maryam. Interfacial fracture toughness of universal adhesive systems treated with an antioxidant. En: Journal of Clinical and Experimental Dentistry, 10 6 2018: 528-536 es
dc.identifier.uri http://hdl.handle.net/10550/67282
dc.description.abstract Background: Secondary caries, degradation of the dentin-resin interface and fracture of the restoration are the most common forms of failure. The aim of this study was to assess the interfacial fracture toughness of three different adhesive approaches and to compare their fracture toughness after surface treatment with antioxidant. Material and Methods: Seventy two dentin blocks with 3×4mm dimension and 3mm thickness were prepared and attached to precured 3×4×12mm composite blocks from both sides. Six adhesive groups (N=12), All-bond universal, Scotchbond universal and Clearfil SE bond with or without antioxidant treatment (Sodium Ascorbate 10% )were applied to dentin surfaces, a 160? polyethylene paper formed the chevron in adhesive-dentin interfaces. Chevron-notched beam fracture toughness was measured following a modified ISO 24370 standard. The uniform composite-dentin-composite block was subjected to a 4-point test in universal machine. Data were analyzed by Kruskal-Wallis, Wilcoxon signed-rank and Mann-Whitney tests (? =0.05). Results: Different adhesive approaches yielded different significant in fracture toughness rates. A significant increase of fracture toughness was observed between adhesive groups after antioxidant surface treatment. The difference in fracture toughness between Scotchbond universal and All-bond universal were significant. Conclusions: The highest value of fracture toughness was reported for Clearfil SE bond and the lowest value was found for All-bond universal. Sodium ascorbate as antioxidant surface treatment had a significant effect in increasing the fracture toughness. es
dc.title Interfacial fracture toughness of universal adhesive systems treated with an antioxidant es
dc.type journal article es_ES
dc.subject.unesco UNESCO::CIENCIAS MÉDICAS es
dc.identifier.doi 10.4317/jced.54188 es
dc.type.hasVersion VoR es_ES

Visualització       (1.085Mb)